Performance item |
Test condition [state] |
Test method |
Test data |
Data unit |
physical property |
proportion |
|
ISO 1183 |
1.27 |
g/cm3 |
Mold shrinkage |
- |
2mm,Parallel |
ISO 294-4 |
1.3 |
% |
- |
2mm,Vertical |
ISO 294-4 |
1.8 |
% |
Water absorption rate |
- |
23℃,24hrs |
ISO 62 |
0.9 |
% |
- |
23℃,50%Humidity |
ISO 62 |
2.0 |
% |
Mechanical properties |
Yield tensile strength |
|
ISO 527 |
60 |
MPa |
Elongation at break |
|
ISO 527 |
60 |
% |
Tensile modulus |
|
ISO 527 |
3500 |
MPa |
Flexural modulus |
|
ISO 178 |
3000 |
MPa |
Bending strength |
|
ISO 178 |
90 |
MPa |
Charpy notched impact strength |
- |
23℃ |
ISO 179 |
5.5 |
KJ/m2 |
- |
-30℃ |
ISO 179 |
5.2 |
KJ/m2 |
Electrical properties |
Insulation strength |
|
IEC 60243 |
13 |
KV/mm |
Volume resistivity |
|
IEC 60093 |
3 |
ohm-cm×1015 |
Thermal property |
Melting point |
|
ISO 3146 |
250 |
℃ |
Hot deformation temperature |
- |
1.82MPa |
ISO 75 |
65 |
℃ |
- |
0.45MPa |
ISO 75 |
186 |
℃ |
Flame retardant |
|
UL94 |
V-0 |
|
|
|
|
|
|
|
|
|
|